Brand Name : YUHONG
Model Number : ASTM B462 UNS N08020 Nickel Alloy 20 Superalloy Flange
Certification : API , ABS, DNV, GL , LR, NK
Place of Origin : CHINA
MOQ : 1PC
Payment Terms : L/C,T/T
Delivery Time : 7 DAYS
Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap
Product Name : Superalloy Pipe Flange
Standard : ASTM B462 / ASME SB462
Material : UNS N08020 Nickel Alloy 20
Size : 1/2"-120"
Process : Forged
Pressure : Class150/300/600/9001500/2500
Flange Face : RF/FF/RTJ
Type : Threaded Flange,Slip On Flange,socket Weld Flange,weld Neck Flange,LAP Joint Flange
Application : Petroleum,chemical,etc,fittings And Connection,beer
ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange
We are one of the biggest projects pipeline products supplier in China, Our products contain steel pipe/tube,fittings, flanges. With development more than 20 years, we have accumulated a great many clients all around the world and Yuhong products also won the great praise among the customers.
Alloy 20 will resist corrosion especially in those environments that contain chemicals like nitric acid, phosphoric acid, chlorides and sulfuric acid. Alloy 20 also has good mechanical properties at both ambient as well as elevated temperatures. Alloy 20 is often termed as a superalloy. ASTM B462/ ASME SB462 Uns N08020 Blind Flange has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides as well as in acidic medium or conditions that contain acidic solutions like sulfuric, phosphoric, and nitric acids.
Alloy 20 Forged and Plate Flange
| ASTM B462 Alloy 20 Slip-On Flange | ASTM B462 Alloy 20 Threaded Flange |
| ASTM B462 Alloy 20 Weld Neck Flange | ASTM B462 Alloy 20 Socket Weld Flange |
| ASTM B462 Alloy 20 Blind Flange | ASTM B462 Alloy 20 Reducing Flange |
| ASTM B462 Alloy 20 Lap Joint Flange | ASTM B462 Alloy 20 Plate Flange |
| ASTM B462 Alloy 20 Orifice Flange | ASTM B462 Alloy 20 Forged Flange |
| ASTM B462 Alloy 20 Ring Type Joint Flange | ASTM B462 Alloy 20 Square Flange |
Alloy 20 Flanges Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS | AFNOR | EN |
| Alloy 20 | 2.4660 | N08020 | Z2NCUD31-20AZ | NiCr20CuMo |
Mechanical Properties
| Alloy | Tensile Strength, min. | Yield Strength, min. | Elongation, min. | Reduction of Area, min. | ||
|---|---|---|---|---|---|---|
| ASTM B462 | ksi | MPa | ksi | MPa | % | % |
| UNS N08020 | 80 | 551 | 35 | 241 | 30.0 | 50.0 |
*All values shall be measured at room temperature.
*Alloy 20 flanges shall be supplied in stabilized-annealed condition.
Chemical Composition
| Element | Wt, % |
|---|---|
| Carbon [C] | ≤0.07 |
| Manganese [Mn] | ≤2.00 |
| Phosphorus [P] | ≤0.045 |
| Sulfur [S] | ≤0.035 |
| Silicon [Si] | ≤1.00 |
| Nickel [Ni] | 32.00~38.00 |
| Chromium [Cr] | 19.00~21.00 |
| Molybdenum [Mo] | 2.00~3.00 |
| Copper [Cu] | 3.00~4.00 |
| Niobium+Tantalum [Nb+Ta] | 8xCarbon~1 |
| Iron | Remainder |
*The tabulated values are abstracted from ASTM B462 Gr. UNS N08020.
ASME SB462 Alloy 20 Slip on Flange Vs DIN 2.4660 Weld Neck Flange
The ASME SB462 Alloy 20 Slip on Flange is slipped into the pipe and then the connection is made with the help of double weld- one on the backside of the flange and one in the front. Generally, the slip on flanges are more affordable than the weld neck flanges, but it can become expensive with the number of welding and inspections. Also, the strength of the slip on flange under any internal pressure is around 2/3rd, and fatigue strength is around 1/3rd of that of the weld neck flange
The DIN 2.4660 Weld Neck Flange is easily recognizable by the tapered hub which comes from the bolted connection to the pipe. The connection is made here with the help of but twelding, and that helps in preventing any type of turbulence at the joint. It also minimizes erosion and reduces restriction in the product flow. The alloy 20 weld neck flanges offer enhanced strength under different types of environments.
Application

|
|
ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange Images |